Stock List
We will satisfy your needs.
- We will offer any size & shape (disk, ring, profiled plate) required.
- We will newly produce any material for any size that are not listed below.
- Usually our stock are based on ASTM specifications. (AMS, ASME, JIS are also available)
- Needless to say, we keep an inventory of individual heat numbers and control the materials remaining after cutting.
Stock list of Sheets (Plates)
A=Available, N/A=Not Available |
Standard size of stock (mm) / material |
Corrosion Resistant Alloys |
Heat Resistant Alloys |
| thickness |
width |
length |
MA276
(N10276) |
MA22
(N06022) |
MA-B2
(N10665) |
MAT21
(N06210) |
MA23
(N06230) |
MA600
(N06600) |
| 1.0 |
1,220 |
3,070 |
A |
A |
N/A |
N/A |
N/A |
N/A |
| 1.6 |
1,220 |
3,070 |
A |
A |
N/A |
N/A |
N/A |
N/A |
| 2.0 |
1,220 |
3,070 |
A |
A |
A |
A |
N/A |
N/A |
| 3.0 |
1,300 |
3,070 |
A |
A |
A |
A |
A |
A |
| 4.0 |
1,300 |
3,070 |
A |
A |
A |
A |
N/A |
N/A |
| 5.0 |
1,300 |
3,070 |
A |
A |
A |
A |
N/A |
N/A |
| 6.0 |
1,300 |
3,070 |
A |
A |
A |
A |
A |
A |
| 8.0 |
1,300 |
3,070 |
A |
A |
A |
A |
N/A |
N/A |
| 10.0 |
1,300 |
3,070 |
A |
A |
A |
A |
N/A |
N/A |
| 12.0 |
1,220 |
3,070 |
A |
A |
A |
A |
N/A |
N/A |
| 16.0 |
1,220 |
3,070 |
A |
A |
N/A |
N/A |
N/A |
N/A |
| 20.0 |
1,000 |
2,000 |
A |
A |
N/A |
N/A |
N/A |
N/A |
| 25.0 |
1,000 |
2,000 |
N/A |
A |
N/A |
N/A |
N/A |
N/A |
| 30.0 |
1,000 |
2,000 |
N/A |
A |
N/A |
N/A |
N/A |
N/A |
|
We will newly produce any material for any size that are not listed below.
Stock list of Bars
A=Available, N/A=Not Available |
| size/material |
MA276 |
MA22 |
MA-B2 |
MAT21 |
| 10φ×1,000L |
A |
A |
A |
A |
| 12φ×1,000L |
A |
A |
A |
A |
| 16φ×1,000L |
A |
A |
A |
A |
| 18φ×1,000L |
A |
A |
N/A |
A |
| 20φ×1,000L |
A |
A |
A |
A |
| 22φ×1,000L |
A |
A |
N/A |
A |
| 25φ×1,000L |
A |
A |
A |
A |
| 30φ×1,000L |
A |
A |
A |
A |
| 35φ×1,000L |
A |
A |
A |
A |
| 40φ×1,000L |
A |
A |
A |
A |
| 45φ×1,000L |
A |
A |
A |
A |
| 50φ×1,000L |
A |
A |
A |
A |
| 55φ×1,000L |
A |
A |
A |
N/A |
| 60φ×1,000L |
A |
A |
A |
N/A |
| 70φ×1,000L |
A |
A |
A |
N/A |
| 80φ×1,000L |
A |
A |
A |
A |
| 90φ×1,000L |
A |
A |
N/A |
N/A |
| 100φ×1,000L |
A |
A |
A |
N/A |
| 110φ×1,000L |
A |
A |
N/A |
N/A |
| 120φ×1,000L |
A |
A |
A |
N/A |
| 130φ×1,000L |
A |
A |
N/A |
N/A |
| 140φ×1,000L |
A |
A |
N/A |
N/A |
| 180φ×1,000L |
A |
A |
N/A |
N/A |
|
We will newly produce any material for any size that are not listed below.
Stock list of Welding Wires
A=Available, N/A=Not Available |
| size/material |
MA276 |
MA22 |
MAT21 |
MA23W |
| 1.6φ×1,000L |
A |
A |
A |
A |
| 2.4φ×1,000L |
A |
A |
A |
A |
| 3.2φ×1,000L |
A |
A |
A |
A |
| 4.0φ×1,000L |
N/A |
A |
N/A |
N/A |
|
We will newly produce any material for any size that are not listed below.